HVOF Plasma Spraying Coating Superalloy Powders

HVOF Plasma Spraying Coating Superalloy Powders

HVOF Plasma Spraying Coating Superalloy Powders We can produce HVOF Powder, Plasma Powder, Superalloy Powder, Plasma Powders, which can be used for Bonding layer for WC coatings, Pulp-making pumps, power generation boilers, parts in a corrosive environment containing vanadium and sulfur,...

HVOF Plasma Spraying Coating Superalloy Powders

Powder

Chemical Composition

Mesh

Typical Application

C

Cr

Si

W

Fe

Mo

Ni

Co

Mn

Nb

NiCr


20.00



5.00Max


Bal


0.5Max


HVOF

≦45μm

Bonding layer for WC coatings

NiCr20

0.20Max

20.00

1.00


0.50Max


Bal


0.5Max


HVOF

53-20μm

Bonding layer for WC coatings

NiCr50

1.00Max

50.00

1.00


0.50Max


Bal


0.5Max


Plasma Spraying

106-45μm

Pulp-making pumps, power generation boilers, parts in a corrosive environment containing vanadium and sulfur

Ni625

0.10

20.0-23.0

/

/

5.00

8.0-10.0

Bal

/

/

3.15-4.15

HVOF

53-20μm

Parts subject to seawater corrosion, such as, in aerospace or aeronautical industry and chemical processing

Ni-C

0.10

16.50

0.90

4.50

5.50

17.00

Bal

2.0Max

0.90


HVOF

53-20μm

Paper-making machine

Ni-SuperC

0.05Max

23.00




18.00

Bal




HVOF

53-20μm

Paper-making machine

Ni276

0.01Max

15.50

0.03

4.00


16.00

Bal

2.5Max

1.00


HVOF

53-20μm

Parts subject to corrosion and high temperature oxidation

Mn400

0.15Max


1.25


1.50

Ti:2.00

Bal


3.50


HVOF

53-20μm

Chemical or petrochemical processing equipment parts

We can produce HVOF Powder, Plasma Powder, Superalloy Powder, Plasma Powders, which can be used for Bonding layer for WC coatings, Pulp-making pumps, power generation boilers, parts in a corrosive environment containing vanadium and sulfur, Pulp-making pumps, power generation boilers, parts in a corrosive environment containing vanadium and sulfur, Paper-making machine, Parts subject to corrosion and high temperature oxidation, Chemical or petrochemical processing equipment parts.

image001(001).jpg

Pulp-making pumps


image003(001).jpg

Power generation boilers


image005.jpg

Parts subject to seawater corrosion in aerospace industry


image007(001).jpg

Parts subject to seawater corrosion in aeronautical industry


image009(001).jpg

Parts subject to seawater corrosion in chemical processing


image011(001).jpg

Paper-making machine


image013(001).jpg

image015(001).jpg

Chemical or petrochemical processing equipment parts


Modern testing Equipment

AmericaThermoFisher ICAP6300

铸宇(001).jpg


United KingdomMarlvin Mastersizer300

铸宇1(001).jpg


LECOCS-230 Carbon/Sulphur Analyzer

铸宇2(001).jpg

TC400C

铸宇3(001).jpg

Global Fusion Technology Team:

The technical team is co-founded with Mr. Yeren Qian (Government Allowance of the State Council) and six experts in metallurgy materials as it’s core. Introduce and absorb international advances in technology and production facilities from America, France and Germany.

There 60 employees at present, including 20 employees with college degree or above ,  12 engineering and technical personnel, 8 executives, 4 senior technicians, 2 intermediate technicians.

23.png

FAQ

1.Q. Why choose US?

(1)We have an experienced technical team understanding different applications. So we can give best advice to our customer about choosing materials and process.

(2).For more than 50 years' development,

● Gas atomized system is used for alloy powder production.

● Powder is carefully screened.

● Accurately control the chemical and particle size.

● Product quality is very consistent.

● Customization is accepted.

2.Q.What is the MOQ ?
A. No MOQ for our existing stock, for special size, MOQ is 5 KGS.
3.Q. Can I place a mixed order?
A. Sure!
4.Q. Can I get a lower price if I order large quantities?
A. Yes, big order get big discount.
5.Q. Do you provide samples ? Is it free or extra ?
A. Yes, we will send you sample before mass production, and start production by your approval. Most sample is free,  you only need to pay the freight.
6.Q. When you ship my order?
A. Normally 7-18 days after receiving your payment, but it can be negotiated based on order qty and production schedule.
7.Q. If I need any products hurry, could you make them fast for me?
A. Yes. If you are hurry, we will make the products as fast as we can and delivery them in the fast shipment.
8.Q. How can you guarantee the production quality ?
A. Our production is based on ISO9001,we have more than 40 years experience of QC team and strictly quality control system in our production process. At the same time,before sent the products, we will sent the free sample for you to test.
9.Q. What about the package?
A. It can make as the you need and depend on the products shapes. Generally, we can provide iron drum, carton, wooden case, and bag packages.


About Delivery and shipping                                 

1. For the products which we have raw material in stock.

               

We can deliver the products within 7-10 days after the payment has been confirmed.

 

We will choose the shipping way as you required: By sea, by air, by express, etc.

 

As for the costs and shipping period information, please contact us via telephone, mail or online trade manager.

 

2.For the products need to start from smelting

                

We will finish the production within 20-25 days after the deposit has been confirmed. We will choose the shipping way as you required:  By sea, by air, by express, etc.

 

As for the costs and shipping period information, please contact us via telephone, mail or online trade manager.

 

Contact Us

Contact: Antonio Fu

Mob: +8613817361629

Email: aj.fu@zhuyualloy.com

Website: www.alloyconsumables.com


Inquiry
Local Business Directory, Search Engine Submission & SEO Tools